Key Specifications
Gold Label IX Extra
Powder / Liquid ratio (g/g)- 0.40 / 0.12
Mixing Time(sec.)- 10
Working Time(min., sec.)- 1.15
Net Setting Time(min., sec.)-2.00
Final Finishing Commencing Time(37°C, after starting mix)
(min., sec.)- 2.30
Gold Label IX
Mixing Time(sec.)- 30
Working Time(min.)-2.0
Finishing begins from the start of the mix(min.)-6
Powder / Liquid Ratio (g/g)- 3.6 / 1.0
Direction To Use
1. POWDER AND LIQUID DISPENSING
- The standard powder-to-liquid ratio is 3.4g/ 1.0g. (1 level scoop of powder to 1 drop of liquid).
- For accurate dispensing of powder, lightly tap the bottle against the hand. Do not shake or invert.
- To dispense the correct amount of liquid from the bottle turn the bottle upside down, keep the nozzle away from the mixing pad and gently press the bottle. Discard the first 1-2 drops after opening a new bottle as the dispensed amount may not be accurate.
- Close bottles tightly immediately after use.
2. MIXING
- Dispense powder and liquid onto the pad. Using the plastic spatula, divide the powder into 2 equal parts. Mix the first portion with all the liquid for 10 seconds. Incorporate the remaining portion and mix the whole thoroughly for 15-20 seconds (Fig. 1).
3. RESTORATIVE TECHNIQUE
- Prepare the tooth using standard techniques. Extensive mechanical retention is not necessary. For pulp capping, use calcium hydroxide.
- Apply GC CAVITY CONDITIONER (10 seconds) or GC DENTIN CONDITIONER (20 seconds) to the bonding surfaces using a cotton pellet or sponge (Fig. 2).
- Refer to the respective instructions for use.
- Rinse thoroughly with water. Dry by blotting with a cotton pellet or gently blowing with an air syringe. DO NOT DESICCATE. The best results are obtained when prepared surfaces appear moist (glistening) (Fig. 3).
- Mix the required amount of GC Gold Label IX GP-EXTRA. Working time is 2 minutes from the start of mixing at 23°C (73.4°F). Higher temperatures will shorten working time.
- Transfer cement to the preparation using a syringe or other suitable instrument. Avoid air bubbles.
- From the preliminary contour and cover with a matrix if required (Fig. 4). g) When set, immediately apply GC Fuji VARNISH (blow dry) or GC Fuji COAT LC (light cure for 10 sec.).
4. FINISHING
- Final finishing under water spray using standard techniques can begin at 6 minutes after starting the mix.
- Apply a final coat of G-COAT PLUS and light cure for 20 sec. (Fig.5, 6). Alternatively, apply GC Fuji VARNISH (blow dry) or GC Fuji COAT LC (light cure for 10 sec.)
- Instruct the patient not to apply pressure for 1 hour.
Packaging
Additional Info
Country Of Origin: Japan
Manufacturer: GC